A crack in the brick on your house is easy to spot and hard to judge. Some cracks are old, stable and mostly cosmetic. Others are a sign that the wall is still moving, or that water is getting in and making things worse every winter. On older Richmond homes, the difference usually comes down to where the crack is, what shape it has and whether it is growing.

This guide explains the common crack patterns homeowners notice, what they can point to, and what a professional repair involves.

Not every crack is a structural emergency

The National Park Service defines cracking in masonry as narrow fissures, roughly 1/16 to 1/2 inch wide, and notes that it can come from several conditions: settlement of the building, mortar that is too hard for the masonry, or the nature of the material itself. Its guidance is measured. Small cracks within a single brick may not be serious, while longer and wider cracks running over a larger area may indicate structural problems and should be monitored.

That gives homeowners a useful starting point. A single hairline crack in one brick is a different conversation from a crack that runs through several courses, opens wider at one end or keeps coming back after it has been patched.

Common crack patterns and what they can mean

The pattern of a crack is one of the best clues to its cause. These are the ones homeowners most often ask about:

  • Stair-step cracks through the mortar joints. A crack that zigzags up through the bed and head joints often follows the path of least resistance through the mortar. The Brick Industry Association (BIA) notes that foundation settlement can cause diagonal or stepped cracking in brickwork directly above the foundation, and that differential settlement, where one part of a structure settles more than another, can also cause cracking.

  • Cracks that are wider at one end. BIA explains that deflection and settlement cracks can be identified by their tapering shape. A crack that is wide at the top and narrows to nothing, or the reverse, suggests something has moved or sagged rather than simply shrunk.

  • Cracks at the corners of windows and doors. BIA describes diagonal cracks in brickwork between windows or doors that usually run from the head or sill of the opening, caused by movement in the wall. A crack that starts at the end of the lintel over a window is also worth a closer look, because BIA notes that an undersized lintel can deflect and crack the brick it supports.

  • Cracks next to rusting metal. Water that reaches steel embedded in masonry, such as lintels or wall ties, can cause it to corrode. BIA notes that rust takes up far more volume than the original steel and can crack or spall the surrounding brick, which then lets in more water.

  • Cracks through the brick faces themselves. When cracks run through the bricks instead of the joints, the mortar may be harder than the brick around it. The National Park Service warns that mortar stronger than the masonry units cannot give, so stresses are relieved through the bricks instead, causing cracking and spalling that cannot be repaired easily. This can happen where older brick has been repointed with modern hard mortar. Our article on why lime mortar matters for historic Richmond brick explains why.

  • Hairline cracks along the edge of the mortar. Fine cracks where the mortar meets the brick often mean the bond has broken. The National Park Service notes that this lets water penetrate, but it is easier to correct with repointing than damage to the bricks themselves.

Signs a crack needs attention soon

A crack is more likely to need prompt professional attention if you notice any of the following:

  • It has grown longer or wider over weeks or months.

  • It runs through many courses of brick or across a large area of wall.

  • The wall on one side of the crack sits out of line with the other side, or a section of wall is bulging.

  • Bricks near the crack are loose, missing or flaking.

  • Windows or doors near the crack have started sticking.

  • You see damp patches, staining or damaged plaster on the inside of the same wall.

  • The crack is on a chimney, where loose masonry and water entry can lead to bigger repairs.

The National Park Service recommends monitoring larger cracks. A dated photo with a tape measure in the frame is a simple way to show a mason whether a crack is changing.

Why patching the crack is not the whole repair

It is tempting to fill a crack with caulk or a tube of mortar repair and move on. The National Park Service cautions that caulking should not be used as a substitute for mortar in repointing. More importantly, its repointing guidance states that it is wrong to assume repointing alone will solve problems caused by something else. Leaking roofs or gutters, differential settlement, rising damp and extreme weather exposure should be dealt with before the masonry work, or the deterioration will continue and the repair will be wasted.

In practice, that means the first job is figuring out why the wall cracked. If the cause is ongoing foundation or structural movement, an evaluation by a structural engineer may be needed before any masonry repair makes sense. The National Park Service also notes that on historic buildings, a consultant such as a historic architect or architectural conservator can help analyze the causes of deterioration.

What professional crack repair can involve

Once the cause is understood and any movement has been addressed, repairs on an older brick home usually combine some of the following:

  1. Raking out and repointing cracked joints with mortar that is compatible with the original brick, usually a softer, lime-rich mix on historic walls. See our brick repointing and tuckpointing service.

  2. Cutting out and replacing cracked or broken bricks. The National Park Service generally prefers replacing damaged units with matching material where suitable brick is available. Learn more about our brick repair work.

  3. Rebuilding loose or badly cracked sections, such as the area around a window head or the top of a garden wall, where patching alone would not hold.

  4. Repairing chimney masonry when cracks show up in the stack, crown or mortar joints. See our chimney repair service and our article on cracked chimney crowns.

  5. Pointing out water sources such as gutters, downspouts and grading, so the repaired wall stays dry.

If the bricks around a crack are already flaking, our guide to spalling brick on older Richmond homes covers that damage, and our historic masonry restoration page explains how we approach older walls.

Cracked brick on older homes around Richmond

Much of Richmond's older housing stock, from rowhouses in the Fan District and Museum District to homes in Church Hill and Ginter Park, is built of softer brick laid in lime-based mortar. Those walls can be very durable, but they can be damaged by hard modern repointing and by repairs that seal a crack without fixing the cause. Older brick homes in the West End and across Henrico face the same questions, especially around chimneys, window openings and foundations.

Getting a crack looked at while it is small is usually far simpler than rebuilding a section of wall after water and movement have had a few more seasons to work on it.

Get a free estimate from Richmond Masonry

Richmond Masonry is a family-owned residential masonry restoration company led by a third-generation mason with over 35 years of experience. We are fully insured, and all of our work carries a five-year guarantee. If you have cracks in your brick walls, chimney or steps and want to know what they mean, we can take a look and recommend the right repair.

Request a free estimate or call 804-836-0517. We are available 7 AM to 7 PM, seven days a week.

Sources

 
 
 

Recent Posts

See All

Comments


Post: Blog2_Post
bottom of page